Study on Leaching Process of Arsenic from Antimony Oxide Powder
           
View Full Text  View/Add Comment  Download reader
DOI:doi:10.3969/j.issn.1007-7545.年份.期号.顺序号
KeyWord:Antimony,Arsenic,Sodium carbonate,Leaching rate
FAN Li-feng~1,XIE Gang~1,YANG Da-jin~2,ZHOU Jian-yong~1
Hits: 2359
Download times: 104
Abstract:
      The mineral phase of arsenic in antimony oxide powder is investigated, according to the property of As_2O_3,the arsenic is transformed to sodium arsenate using the following process: roasting with sodium carbonate in high temperature,de-arsenic with carbonic acid,vacuum filtering and water-washing.The factors that influenced leaching rate of arsenic are discussed.The leaching rate of arsenic is above 94% on the optimized condition.