| Study on Tellurium-Bearing Waste Residue with Oxidation Leaching |
| |
| View Full Text View/Add Comment Download reader |
| DOI:doi:10.3969/j.issn.1007-7545.年份.期号.顺序号 |
| KeyWord:Copper anode slimel Tellurium; Leaching; Oxidant |
| LI A-lin,CHENG Li-li,LIU Jian-hua,LIAO Chun-fa |
|
| Hits: 2017 |
| Download times: 28 |
| Abstract: |
| Based on the characteristic of refractory tellurium-bearing waste residue after extracting noble metals in certain factory, the tellurium leaching rate of general basic leaching process is only less than 10%, the tellurium leaching rate is less than 79% using hydrogen peroxide oxidation leaching in sulfuric acid and sodium chloride solution. But it can improved evidently by using a new craft of potassium permanganate oxidation leaching in sulfuric acid solution at normal temperature. The experiment results show that the tellurium leaching rate can reach 92% after leaching 5 hours. |