| Indium Extraction by Sulfuric Acid Pressure-Oxidation Leaching Process from Tin Dust with Indium |
| Received:May 18, 2011 |
| View Full Text View/Add Comment Download reader |
| DOI:doi:10.3969/j.issn.1007-7545.2011.12.010 |
| KeyWord:Tin dust; Indium; Leaching; Sulfuric acid; Pressure-oxidation leaching |
| Author | Institution |
| HUANG Ying-hong1, WANG Ya-xiong2, WANG Wei-chang1 |
1.云南锡业集团,云南个旧 ;2.昆明贵金属研究所,昆明 |
|
| Hits: 2811 |
| Download times: 37 |
| Abstract: |
| Sulfuric acid pressure-oxidation leaching process from tin dust with indium was studied. Effects of various factors on leaching had been investigated. The results show that leaching rate of indium can reach 93. 66% under the conditions including ratio of liquid to solid of 4∶1, H2SO4 initial concentration of 150 g/L, leaching temperature of 150 ℃, oxygen partial pressure of 0.7 MPa, and leaching time of 150 min. |
| Close |