| Experimental Study on Reductive Volatilization of In-Fe Residue |
|
Received:June 15, 2012
Revised:June 20, 2012
Accepted:June 25, 2012
Published Online:November 26, 2012
|
| View Full Text View/Add Comment Download reader |
| DOI:10.3969/j.issn.1007-7545.2012.12.010 |
| KeyWord:indium-rich zinc acid-leaching residue; reductive smelting; volatilization |
| Author | Institution |
| lixuguang |
桂林理工大学南宁分校 |
| liuPing |
桂林理工大学南宁分校 |
| liangduoqiang |
广西大学资源与冶金学院 |
| Tao Zheng-Xin |
来宾华锡冶炼有限公司 |
|
| Hits: 2495 |
| Download times: 2309 |
| Abstract: |
| The indium-rich zinc acid-leaching residue with 0.046% of indium and 50% of iron was reductively volatilized in a rotary furnace. The results indicate that the evaporation rate of indium can reach 67.56% under the conditions including particle size of In-Fe slag of -3 mm, proportion of granular coal of 30%, feed speed of 200 kg/h, kiln rotational speed of 3 r/min, volatilization temperature of 1 250 ℃, and air coefficient of 1.1. |