Column Leaching of Zinc Oxide Ore in NH3-NH4Cl-H2O System
Received:May 21, 2013   Revised:May 23, 2013   Accepted:May 24, 2013      Published Online:October 25, 2013
View Full Text  View/Add Comment  Download reader
DOI:10.3969/j.issn.1007-7545.2013.11.002
KeyWord:zinc oxide ore; NH3-NH4Cl-H2O system; column leaching
              
AuthorInstitution
Wang Rui-xiang 江西理工大学 冶金与化学工程学院
Yu Pan 江西理工大学 冶金与化学工程学院
Zeng Bin 江西理工大学 冶金与化学工程学院
Wang Zhi-gang 中国瑞林工程技术有限公司
Ruan Jian-guo 中国瑞林工程技术有限公司
Hits: 2196
Download times: 2939
Abstract:
      Zinc oxide ore was column leached in NH3-NH4Cl-H2O system. The results show that the leaching rate of zinc is 92.19% and zinc ion concentration in leachate is 54.38 g/L under the conditions including ore particle size of 0.1~10 mm, double column series operation, ore loading in first column of 2 629 g and 1 314 g in second column, total ammonia concentration of 7.5 mol/L, NH4Cl/NH3=2∶1, and leaching time of 30 days. Compared with the results of bottle leaching, zinc leaching rate of column leaching is improved by about 4 percent point and zinc ion concentration in leachate is improved by about 11 g/L.