Study on Reduction Experiment of Lead-rich Slag
Received:May 27, 2013   Revised:May 28, 2013   Accepted:May 28, 2013      Published Online:August 22, 2013
View Full Text  View/Add Comment  Download reader
DOI:10.3969/j.issn.1007-7545.2013.09.003
KeyWord:lead-rich slag; crude lead; reduction; coal
  
AuthorInstitution
fan yan qing 北京矿冶研究总院
Hits: 2598
Download times: 3060
Abstract:
      The reduction of lead-rich slag from oxidation bottom blowing furnace was conducted by adding coal. The effects of ratio of coal to lead-rich slag, reduction time and temperature, and ratio of CaO/SiO2 and Fe/SiO2 on reduction were studied. The lead content in slag is below 2% and zinc content in slag is above 85% under the optimum conditions including coal ratio of 3.25%~3.50% at reduction temperature of 1 225 ℃ for 30 min.