Experimental Study on Selective Arsenic Removal from High Arsenic Bearing Lead Anode Slime
Received:October 22, 2013   Revised:October 23, 2013   Accepted:October 28, 2013      Published Online:April 22, 2014
View Full Text  View/Add Comment  Download reader
DOI:10.3969/j.issn.1007-7545.2014.05.002
KeyWord:high arsenic bearing lead anode slime; selective; arsenic removal
           
AuthorInstitution
qin xiao long 郴州市金贵银业股份有限公司
xie zhao feng 郴州市金贵银业股份有限公司
liuwanli 郴州市金贵银业股份有限公司
tan lin 郴州市金贵银业股份有限公司
Hits: 2577
Download times: 2948
Abstract:
      Selective arsenic removal from high arsenic bearing lead anode slime was conducted in alkaline system by feeding air. The effects of dosage of caustic soda, air flow, leaching temperature and time on arsenic removing rate were investigated. The results show that the arsenic removing rate is 95% above under the optimum conditions including dosage of caustic soda of 1.4 times of theoretical value, air flow of 100 L/h, ratio of liquid to solid of 5∶1, leaching temperature of 80 ℃, size of anode slime of 0.15~0.178 mm, and leaching duration of 2 h.