| Separation of Cr3 and Fe3 from Sulphuric Acid Leaching Solution of Chromite |
|
Received:January 22, 2014
Revised:January 24, 2014
Accepted:January 26, 2014
Published Online:June 23, 2014
|
| View Full Text View/Add Comment Download reader |
| DOI:10.3969/j.issn.1007-7545.2014.07.001 |
| KeyWord:chromite; Cr3 ; Fe3 ; separation; acidic solution; sodium jarosite |
| Author | Institution |
| ZHANG Bo |
东北大学 多金属共生矿生态化冶金教育部重点实验室 |
| YANG Dapeng |
东北大学 多金属共生矿生态化冶金教育部重点实验室 |
| ZHAO Qing |
东北大学 多金属共生矿生态化冶金教育部重点实验室 |
| SHI Peiyang |
东北大学 多金属共生矿生态化冶金教育部重点实验室 |
| LIU Chengjun |
东北大学 多金属共生矿生态化冶金教育部重点实验室 |
| JIANG Maofa |
东北大学 多金属共生矿生态化冶金教育部重点实验室 |
|
| Hits: 4181 |
| Download times: 4253 |
| Abstract: |
| The precipitation of iron from acidic solution was investigated by means of hydrolysis method and sodium jarosite method respectively. The results show that hydrolysis method is ineffective while sodium jarosite method can remove iron in acidic solution. The precipitation rate of iron is close to 100% and the loss rate of chromium is 7% below in laboratory test the conditions of pH=-0.87, 165 ℃ with addition of seed crystal of sodium jarosite. |
| Close |