Bioleaching of Uranium Ore from Sand-type Uranium Deposit
Received:April 02, 2014   Revised:April 09, 2014   Accepted:April 10, 2014      Published Online:September 19, 2014
View Full Text  View/Add Comment  Download reader
DOI:10.3969/j.issn.1007-7545.2014.10.013
KeyWord:bioleaching of uranium; acid leaching of uranium; sand-type uranium ore
              
AuthorInstitution
ZHOU Yipeng 中国地质大学
SHEN Zhaoli 中国地质大学
HE Jiangtao 中国地质大学
LIU Jinhui 东华理工大学
SHI Weijun 东华理工大学
Hits: 2263
Download times: 2746
Abstract:
      One sand-type uranium deposit was bioleached with different acidities and Fe3 concentrations. The result was compared with that of acid leaching of 5 g/L H2SO4. The results show that the optimum bioleaching rate of uranium of 96.43% is obtained under the conditions of 4 g/L H2SO4 and 2 g/L Fe3 , which is 27% higher than that of acid leaching with 5 g/L H2SO4. Fe3 concentration over 2 g/L is not effective to promote uranium bioleaching.