| Removal of Fe(III) from Oxygen Pressure Sulfuric Acid Leaching Solution of Pt-Pd Concentrate |
|
Received:November 06, 2014
Revised:November 18, 2014
Accepted:November 19, 2014
Published Online:March 23, 2015
|
| View Full Text View/Add Comment Download reader |
| DOI:10.3969/j.issn.1007-7545.2015.04.001 |
| KeyWord:Pt-Pd concentrate; sulfuric acid leaching solution; removal of Fe(III); extraction; ferroalumen; hematite |
| Author | Institution |
| zhangkuifang |
广州有色金属研究院 |
| liuzhiqiang |
广州有色金属研究院 |
| caohongyang |
广州有色金属研究院 |
| qiuxianyang |
广州有色金属研究院 |
|
| Hits: 2222 |
| Download times: 2892 |
| Abstract: |
| Iron was removed from oxygen pressure sulfuric acid leaching solution of Pt-Pd concentrate by N235 extraction, ferroalumen process, and hematite process respectively. The advantages and disadvantages, cost, and experimental conditions of the three processes were compared. The results show that losses of copper ions and quantity of slag in ferroalumen process and hematite process are both large. Extraction process is worth of further development considering its advantages of small loss of valuable metals and zero-slag produce. |