Effect of Heat Treatment on Structure and Hydrogen Storage Property of La0.53Ce0.47Ni3.4Co0.6Mn0.3Cu0.1 Alloy
Received:December 16, 2015   Revised:December 28, 2015   Accepted:December 29, 2015      Published Online:May 19, 2016
View Full Text  View/Add Comment  Download reader
DOI:doi:10.3969/j.issn.1007-7545.2016.06.016
KeyWord:heat treatment; hydrogen storage alloy; phase structure; electrochemical properties
                 
AuthorInstitution
caohui 内蒙古科技大学 材料与冶金学院
Liu Zhaogang 内蒙古科技大学 材料与冶金学院
Xu Jin 内蒙古稀奥科贮氢合金有限公司
Wang Jianhui 内蒙古科技大学 材料与冶金学院
Luo Qiwen 内蒙古包头稀土研究院;内蒙古包头稀土研究院
Ji Liqiang 内蒙古稀奥科贮氢合金有限公司
Hits: 2123
Download times: 2092
Abstract:
      La0.53Ce0.47Ni3.4Co0.6Mn0.3Cu0.1 alloy was prepared by induction melting and annealed under different temperatures. Phase composition and structure were characterized by XRD, hydrogen storage performance was tested and analyzed by two-electrode cell simulation test system. The results show that with increase of annealing temperature, composition of alloy presents no change, but crystallization degree and grain size increase gradually. Discharge capacity and cycle stability of alloy are improved by annealing treatment, but high-rate discharge capacity of alloy is deteriorated.