Experiment and Industrial Practice of Leaching of Antimony-bearing Gold Concentrate with Alkaline Sulfide
Received:May 11, 2017   Revised:May 12, 2017   Accepted:May 15, 2017      Published Online:August 21, 2017
View Full Text  View/Add Comment  Download reader
DOI:doi:10.3969/j.issn.1007-7545.2017.09.001
KeyWord:sodium sulfide; antimony-bearing gold concentrate; cathode antimony; electrodeposition
           
AuthorInstitution
zhangdawei 北京矿冶研究总院
wangyun 北京矿冶研究总院
jinrangong 北京矿冶研究总院
liyun 北京矿冶研究总院
Hits: 2115
Download times: 2449
Abstract:
      Antimony in antimony-bearing gold concentrates was recovered by alkaline sodium sulphide leaching, and segregation-free electrodeposition. Based on small-scale experiment, industrial practice was carried out according to actual conditions of production site. After optimization of process parameters of electrodeposition, comprehensive leaching rate of antimony is 96.72%, purity of cathode antimony is 96.36%, antimony concentration in barren liquor is 5.54 g/L, comprehensive current efficiency is 63.84%, and NaOH consumption for one ton antimony is 617.2 kg.