| Study on Separation of Arsenic and Tin from High As and Sn Bearing Anode Slime |
|
Received:December 20, 2017
Revised:December 25, 2017
Accepted:December 26, 2017
Published Online:May 17, 2018
|
| View Full Text View/Add Comment Download reader |
| DOI:doi:10.3969/j.issn.1007-7545.2018.06.003 |
| KeyWord:high As and Sn bearing anode slime; alkaline roasting; separation of As and Sn; valuable metals |
| Author | Institution |
| WANG Xiao-yang |
广东环境保护工程职业学院 环境工程系 |
| WANG Wen-xiang |
广东环境保护工程职业学院 环境工程系;广东省固体废弃物资源化与重金属污染控制工程技术研究中心 |
| FANG Hong-sheng |
广东省固体废弃物资源化与重金属污染控制工程技术研究中心 |
| MO Yue-jian |
广东省固体废弃物资源化与重金属污染控制工程技术研究中心 |
|
| Hits: 1846 |
| Download times: 2343 |
| Abstract: |
| High As and Sn bearing anode slime were treated by alkaline roasting and leaching. The effects of mass ratio of soda to anode slime, roasting temperature, roasting time, L/S, leaching temperature, and leaching time on leaching efficiency of metals were investigated. The results show that leaching rate of As is 95.2% and As content in leaching slag is 0.5% below under the optimum conditions including mass ratio of soda to anode slime of 0.9, roasting temperature of 600 ℃, roasting time of 2 h, L/S=3 mL/g, leaching temperature of 80 ℃, and leaching time of 2 h. Other valuable metals in anode slime are relatively enriched for further recycling. |
| Close |
|
|
|