| Antimony Recovery from Antimony Sulfide Slag with Vacuum Evaporation |
|
Received:December 04, 2018
Revised:December 07, 2018
Accepted:December 10, 2018
Published Online:February 15, 2019
|
| View Full Text View/Add Comment Download reader |
| DOI:doi:10.3969/j.issn.1007-7545.2019.03.003 |
| KeyWord:antimony sulfide slag; vacuum evaporation; separation; recovery; antimony |
| Author | Institution |
| Bao zhi-qun |
昆明冶金研究院,共伴生有色金属资源加压湿法冶金技术国家重点实验室 |
| QIU Ke-qiang |
中南大学化学化工学院 |
|
| Hits: 1995 |
| Download times: 2154 |
| Abstract: |
| Antimony sulfide slag from antimony industrial processes was treated by vacuum evaporation to recover antimony based on characteristics of antimony sulfide slag and theoretical analysis. Effects of particle size of materials, system pressure, evaporation time, and evaporation temperature on evaporation ratio of antimony sulfide slag were investigated. The results show that evaporation ratio is 27.9% and antimony content in distilland reduces to 0.2% with antimony separation efficiency of 98.6% under the conditions including particle size of 0.106~0.075 mm, evaporation temperature of 923 K, evaporation time of 30 min, and system pressure of 50 Pa. |
| Close |