| Effect of Ratio of Soda to Material on Recovery of Valuable Elements from Spent Auto-catalyst with Soda Sintering and Water Leaching Process |
|
Received:January 16, 2019
Revised:January 16, 2019
Accepted:January 18, 2019
Published Online:February 15, 2019
|
| View Full Text View/Add Comment Download reader |
| DOI:doi:10.3969/j.issn.1007-7545.2019.03.017 |
| KeyWord:spent auto-catalyst; PGMs; roasting; ratio of soda to material; water mixing |
| Author | Institution |
| Yan Li |
北京矿冶科技集团有限公司 北京 |
| WANG Guang-hui |
北京矿冶科技集团有限公司 北京 |
| LIU Gui-qing |
北京矿冶科技集团有限公司 北京 |
| YAO Xian-zhao |
北京矿冶科技集团有限公司 北京 |
|
| Hits: 1906 |
| Download times: 1689 |
| Abstract: |
| Effects of ratio of soda to material with water mixing on recovery of PGMs, RE and aluminum from spent auto-catalyst by roasting with soda and water leaching process were investigated. PGMs are enriched 9.97 times and cerium recovery is 68% above after roasted with soda and leached with water. Content of Al and Si in water washing solution is 10 g/L above, which can be used to prepare polyaluminium sulfate flocculant. |