Study on Smelting of High Carbon Ferrochrome with Microwave Heating
Received:August 03, 2020   Revised:August 12, 2020   Accepted:August 14, 2020      Published Online:October 31, 2020
View Full Text  View/Add Comment  Download reader
DOI:doi:10.3969/j.issn.1007-7545.2020.11.015
KeyWord:microwave heating; carbon allocation; slag allocation; recovery rate
                 
AuthorInstitution
ZHAO Zhi-min 中国钢研科技集团 新冶高科技集团有限公司
PANG Jian-ming 中国钢研科技集团 新冶高科技集团有限公司
FANG Jian-feng 中国钢研科技集团 新冶高科技集团有限公司
DI Jiu-hai 中国钢研科技集团 新冶高科技集团有限公司
LI Shi-wen 中国钢研科技集团 新冶高科技集团有限公司
HE Jia-qing 中国钢研科技集团 新冶高科技集团有限公司
Hits: 1763
Download times: 1966
Abstract:
      In order to develop a new clean and efficient high-carbon ferrochrome smelting process, experiments of microwave heating chrome ore pellets to smelt high-carbon ferrochrome were carried out. Influence of proportion of carbon and slag allocation on recovery rate of chromium was investigated. The results show that microwave heating of chromium ore pellets for 100 to 120 minutes can reach a high-carbon ferrochrome smelting temperature of 1 550—1 620 ℃, and obtain high-carbon ferrochrome that meets the requirements of national standards with chromium recovery rate of 94% above. When carbon allocation coefficient is 1.1 and silica is added to make slag R=SiO2/(MgO+Al2O3)=0.55, the smelting effect is the best. When R value is lower, chromium content in alloy and recovery rate are significantly reduced, which can be improved by prolonging microwave heating time.