Research on Recovery of Lithium from Lepidolite Concentrate by Chlorination Roasting and Water Leaching
Received:October 17, 2020   Revised:October 19, 2020   Accepted:October 25, 2020      Published Online:January 21, 2021
View Full Text  View/Add Comment  Download reader
DOI:doi:10.3969/j.issn.1007-7545.2021.02.011
KeyWord:lepidolite; chlorination roasting; water leaching; recovery of lithium
                 
AuthorInstitution
LIU Lin 中国地质科学院郑州矿产综合利用研究所
LIU Lei 中国地质科学院郑州矿产综合利用研究所
ZHANG Liang 中国地质科学院郑州矿产综合利用研究所
WANG Wei 中国地质科学院郑州矿产综合利用研究所
LIU Hong-zhao 中国地质科学院郑州矿产综合利用研究所
CAO Yao-hua 中国地质科学院郑州矿产综合利用研究所
Hits: 2044
Download times: 1903
Abstract:
      Lithium was recovered from lepidolite concentrate with 3.23% Li2O by chlorination roasting and water leaching method. Effects of chlorination agent dosage, roasting temperature, roasting time, L/S, leaching temperature and leaching time on Li2O leaching rate were discussed. The results show that leaching rate of Li2O is 95.36% under the optimum conditions including CaCl2 dosage of 3/4 of mineral mass, roasting temperature of 900 ℃, roasting time of 40 min, L/S of leaching of 3︰1, and leaching time of 40 min under room temperature.
Close