New Technology of Two-stage Pressure Leaching of Nickel Extraction from Nickel Laterite Ore
Received:June 14, 2024   Revised:August 05, 2024   Accepted:August 06, 2024      Published Online:September 11, 2024
View Full Text  View/Add Comment  Download reader
DOI:doi:10.3969/j.issn.1007-7545.2024.10.003
KeyWord:nickel laterite ore; pressure leaching; high pressure acid leaching; nickel
           
AuthorInstitution
ZHENG Chaozhen 矿冶科技集团有限公司
LIU Sanping 矿冶科技集团有限公司
WANG Haibei 矿冶科技集团有限公司
JIANG Kaixi 矿冶科技集团有限公司
Hits: 1419
Download times: 1548
Abstract:
      Two-stage pressure leaching process is proposed to extract Ni from limonite-type and saprolite-type nickel laterite ore. The recommended conditions for the first stage high pressure acid leaching include acid ore ratio of 330 kg/t, temperature of 250 ℃, slurry solid content of 30% and reaction time of one hour. The recommended conditions for the second stage pressure leaching include temperature of 230 ℃, reaction time of one hour and slurry solid content of 35%., The nickel extraction rate of first stage high pressure acid leaching and second stage pressure leaching is 97.58% and 83.96% respectively, and the total nickel leaching rate is 93.81%, which greatly improves the utilization rate of nickel laterite ore resources. The Fe and Al concentration in solution can be reduced to below 1 g/L, which can reduce the amount of alkali used in subsequent neutralization processes.